Spatial atomic layer deposition system

Summary of the technology

University of Waterloo (UW) researchers have developed a novel commercial-scale AP-SALD system that aims to upscale lab devices (~1 cm2) to commercial-scale devices (>232 cm2) while maintaining and improving their efficiency, stability, and uniformity. This system enables high-throughput manufacturing that facilitates the commercialization of next generation nanomaterials.

University of Waterloo
University of Waterloo

Background

Atomic layer deposition (ALD) is the best technique for producing films with nanometer-scale thickness control, as it deposits a film one atomic layer at a time. As feature sizes continue to decrease in applications such as integrated circuits and memory devices, ALD is becoming the only option for depositing some thin-film components which are not possible using CVD and PVD processes. Conventional ALD operates by sequentially inserting two chemical precursor gases into a vacuum chamber, with evacuation and purge steps in between the exposures. A single atomic layer of the material is formed after each sequence, and the sequence is repeated multiple times to build up a film. Hence conventional ALD separates the two precursor gases in time. In contrast, spatial atomic layer deposition (SALD) techniques have been developed, which separate the two precursors in space, rather than in time. The substrate is moved back and forth between the two precursor gases to replicate the sequential exposures. This eliminates the evacuation and purge steps that make SALD slow. Since it can operate in atmospheric conditions, it is often referred to as atmospheric pressure spatial ALD (APSALD). AP-SALD can produce thin-film layers of materials (typically metal oxides) that are compact and pinhole-free. AP-SALD can deposit thin films at low temperatures (typically 100 to 350°C), is 1-2 orders of magnitude faster than conventional ALD, and is scalable (roll-to-roll compatible).

Advantages

  • Deposition process operates in ambient pressure, eliminating the high operational and capital cost associated with vacuum-based methods in existing ALD, CVD, PVD technologies.
  • Ability to deposit controlled and conformal nanoscale films, including sub-10 nm films as well as films >20 nm thick with ~1 nm resolution.
  • Modular design to allow scaling for high throughput (>1000 wafers/hr possible) and deposition over large areas (i.e., > 15 cm x 30 cm).
  • Capacity to deposit different materials (e.g., SnO2, WO3, Al2O3, AZO…) on a wide range of substrate types, thickness, and geometries.
  • Low temperature deposition is compatible with flexible substrates.

Potential applications

  • Thin film electronics including memory devices, logic chips, power electronics, display technologies, smart fabric, smart windows.
  • Energy storage/generation including batteries, battery electrode, fuel cells, solar cells, thermoelectric devices.
  • Flexible electronics and sensor applications within the automotive, environment and medtech sectors.
  • Emerging devices and MEMS/NEMS, such as nanotube/nanowire devices, graphene/carbon nanotube devices, optoelectronics.

Related Keywords

  • Nanomaterials
  • stability
  • efficiency
  • uniformity
  • spatial atomic layer deposition
  • commercial-scale
  • ap-sald system
  • high-throughput manufacturing
  • lab-to-commercial scaling
  • next-generation devices

About University of Waterloo

The University of Waterloo, renowned for its innovative spirit and co-op education model, excels in cutting-edge research across diverse fields, including advanced manufacturing, artificial intelligence, sustainability, and health technologies.

University of Waterloo

Never miss an update from University of Waterloo

Create your free account to connect with University of Waterloo and thousands of other innovative organizations and professionals worldwide

University of Waterloo

Send a request for information
to University of Waterloo

About Technology Offers

Technology Offers on Innoget are directly posted
and managed by its members as well as evaluation of requests for information. Innoget is the trusted open innovation and science network aimed at directly connect industry needs with professionals online.

Help

Need help requesting additional information or have questions regarding this Technology Offer?
Contact Innoget support